Evaluation of Mechanical Properties of Sputtered Ceramic Films from Nanoindentation and Wafer Curvature Techniques

Published online by Cambridge University Press:  15 February 2011

Rama B. Inturi
Affiliation:
Department of Metallurgical and Materials Engineering, The University of Alabama, Tuscaloosa, AL 35487-0202
John A. Barnard
Affiliation:
Department of Metallurgical and Materials Engineering, The University of Alabama, Tuscaloosa, AL 35487-0202
Get access

Abstract

TiB2, MoSi2, Si3N4 and Ta4N ceramic films were magnetron sputtered on oxidized Si and Coming 7059 glass substrates at ambient temperature. X-ray diffraction studies indicate that the structure of the films is very different on the two substrates, even though the surface of both substrates is amorphous. The hardness and elastic modulii of the films on oxidized Si are slightly higher than those of the films deposited on Coming glass substrate, even at indentation depths where substrate effects are considered to be negligible. A substantial increase in hardness (5–10 GPa) was observed for TiB2 films, when compared to the properties of bulk stoichiometric TiB2. Stress- temperature diagrams determined from room temperature to 250 C indicate that all the films prepared in this study display a pure elastic behavior in that temperature range.

Type
Research Article
Copyright
Copyright © Materials Research Society 1996

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

[1] Deng, H., Chen, J., Inturi, R. B., and Barnard, J. A., in press, Surface Coatings and Technology, 1995 Google Scholar
[2] Scharf, T., Inturi, R. B., and Barnard, J. A., unpublished resultsGoogle Scholar
[3] Deng, H., Inturi, V. R., and Barnard, J. A., in Thin Films - Stresses and Mechanical Properties V, edited by Baker, S.P., Ross, C. A., Townsend, P. H., Volkert, C. A., and Børgesen, P. (Mat. Res. Soc. Symp. Proc. 356, Boston, MA, 1995) pp. 773778 Google Scholar
[4] Chinmulgund, M., Inturi, R. B., and Barnard, J. A., in press, Thin Solid Films, 1995 Google Scholar
[5] Chinmulgund, M., M. S. Thesis, The University of Alabama, Tuscaloosa, AL 1994 Google Scholar
[6] Saha, R., Inturi, R. B., and Barnard, J. A., presented at the MRS Fall 1995 meeting, Boston, MA, 1995 (unpublished)Google Scholar
[7] Chen, J. and Barnard, J. A., Mater. Sci. and Eng. A, A 191, 233 (1995)Google Scholar
[8] Saha, R., Inturi, R. B., and Barnard, J. A., in press, Surface Coatings and Technology, 1995 Google Scholar
[9] Bhushan, B., Gupta, B. K., Handbook of Tribology, 1st edition, (Mc-Graw-Hill Inc., 1991) p4.39, pp. 4.54 - 4.56Google Scholar