Hostname: page-component-55f67697df-2z2hb Total loading time: 0 Render date: 2025-05-11T10:52:59.893Z Has data issue: false hasContentIssue false

Consolidation of Nickel Base Superalloys Powder by Low Pressure Plasma Deposition

Published online by Cambridge University Press:  15 February 2011

R.W. Smith
Affiliation:
General Electric Co. Gas Turbine Division Schenectady, New York 12345
L.G. Peterson
Affiliation:
General Electric Co. Gas Turbine Division Schenectady, New York 12345
W.F. Schilling
Affiliation:
General Electric Co. Gas Turbine Division Schenectady, New York 12345
Get access

Extract

Powder Metallurgy (P/M) technology has seen an important series of advances in the past twenty-five or so years. It has progressed from a press + sinter methodology (which still has important uses) to one of being a complete processing technology where, ultimately, the structure and properties of totally new materials can be synthesized. A key step in this evolution was the application of P/M techniques to high performance materials such as nickel-based superalloys. This effort began in the early 1960's and has resulted in several important commercial applications such as P/M gas turbine disks and shafts.Attention has now turned to the potential use of Rapid Solidification Technology (RST) as a means of furthering the span of materials which can be made available for a wide variety of engineering applications. Rapidly solidified nickel, cobalt, titanium, aluminum and copper based materials are all the subject of extensive research and development at the present time (1).

Type
Research Article
Copyright
Copyright © Materials Research Society 1984

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Mehrabian, R., ed., Rapid Solidification Processing, Principles and Technologies III National Bureau of Standards, Dec., 1982, Gaithersburg.Google Scholar
2. Jackson, M.R., Rairden, J.R., Smith, J.S., and Smith, R.W. in: Journal of Metals Nov. 1981 p. 23.Google Scholar
3. Muehlberger, E.: Seventh International Metal Spraying Conference Proc. London England 1973, Paper No. 58, Welding Institute.Google Scholar
4. Field, R.D. and Fraser, H.L. in: Met. Trans. 1978, 9A, No. 1 pp. 131134.Google Scholar
5. Bricknell, R.H. and Woodford, D.A., General Electric Co., Corporate Research and Development TIS Report No. 82CRD222, August 1982.Google Scholar
6. Siemers, P.A., ed. Third Quarterly Report.Google Scholar