Hostname: page-component-5f56664f6-x5np6 Total loading time: 0 Render date: 2025-05-07T07:21:08.206Z Has data issue: false hasContentIssue false

Fracture Surface Analysis of Ball Bearing Steel by X-Ray Residual Stress Measurement

Published online by Cambridge University Press:  06 March 2019

Hirokazu Nakashima
Affiliation:
NTN Toyo Bearing Co. Ltd., 511 Kuwana, Japan
Noriyuki Tsushima
Affiliation:
NTN Toyo Bearing Co. Ltd., 511 Kuwana, Japan
Hiroshi Muro
Affiliation:
NTN Toyo Bearing Co. Ltd., 511 Kuwana, Japan
Get access

Extract

Plastic deformation necessarily accompanies fracture even in high hardness steels such as ball bearing steel, though it is within a very shallow layer just under the fracture surface. The depth of the plastic deformation zone can he determined by X-ray measurement of half value breadth. However, in the case of high hardness steel, the half value breadth is not changed significantly by this kind of plastic deformation. On the contrary, residual stress on the fractured surface was found to change remarkably depending on the mode of fracture such as static, fatigue or delayed types.

Type
X-Ray Diffraction Stress (Strain) Determination
Copyright
Copyright © International Centre for Diffraction Data 1979

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Taira, S. and Hayashi, K., Trans. of the Iron and Steel Institute of Japan, 8:20 (1968).Google Scholar
2. Kitagawa, H. and Matstunoto, T., Trans, of the Japan Society of Mechanical Engineers, 41:22 (1975).Google Scholar
3. Tsushima, N., Nakashima, H., and Muro, H., J. of the Japanese Society for Strength and Fracture of Materials, 10:91 (1975).Google Scholar
4. Fracture Toughness, ISI Publication 121, p. 55.Google Scholar
5. Borik, F. and Chapman, R. D., Trans. ASM, 53:447 (1961).Google Scholar
6. Williams, M. L., J. Appl. Mech., 24:109 (1957).Google Scholar
7. Fracture Toughness Testing and Its Application, ASTM STP 381, p. 190 (1965).Google Scholar